Quote:
Originally Posted by Dust View Post
the west system is a room temp system and DOES NOT BENEFIT FROM POST CURE. THE TG is 129F and that be it, no improvement available.
You can raise the HDT via postcure (16 hours, ~120 F) to near 140 F per their engineering data. However, it's interesting that this doesn't appear to affect the Tg (onset values) per the info you received. Yikes.

Any materials science folks out there care to explain the relationship (or lack thereof) between HDT and Tg?

D
Reply With Quote
Reply


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -4. The time now is 01:07 AM.


Powered by vBulletin® Version 3.6.7
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.